EVER BEST(HK) LIMITED

One-stop sourcing for global plastic customers.

Become solution partner for our customers.

Home
Products
About Us
Factory Tour
Quality Control
Contact Us
Request A Quote
Home ProductsABS Plastic Raw Material

ABS SH625 with High Flow and High Impact for Ski Flat, Miscellaneous goods,Refrigerator plate, suitcase, bobbin.

ABS SH625 with High Flow and High Impact for Ski Flat, Miscellaneous goods,Refrigerator plate, suitcase, bobbin.

ABS SH625 with High Flow and High Impact for Ski Flat, Miscellaneous goods,Refrigerator plate, suitcase, bobbin.
video
ABS SH625 with High Flow and High Impact for Ski Flat, Miscellaneous goods,Refrigerator plate, suitcase, bobbin.
Product Details:
Place of Origin: Korea
Brand Name: LG CHEM
Certification: MSDS, ROSH,UL
Model Number: SH625
Payment & Shipping Terms:
Minimum Order Quantity: 16T
Price: negotiable according to order quantity
Packaging Details: 25KG/BAG, 40BAGS PER PALLET
Delivery Time: 20 WOKING DAYS UPON RECEIPT OF ORDER CONFIRMATION AND PAYMENT
Payment Terms: T/T
Supply Ability: 500T PER MONTH
Contact Now
Detailed Product Description
Color: Customer Request Shape: Particle
Material: ABS Usage: Electric Parts
Name: SH625 Type: 100% Virgin Material
High Light:

abs plastic granules

,

acrylic butadiene styrene

SH625 EXTRUSION MOLDING GRADE PLASTIC RAW MATERIAL WITH HIGH IMPACT FOR AUTOMOBILE INTERIOR.

ABS SH625 with High Flow and High Impact for Ski Flat, Miscellaneous goods,Refrigerator plate, suitcase, bobbin. 0ABS SH625 with High Flow and High Impact for Ski Flat, Miscellaneous goods,Refrigerator plate, suitcase, bobbin. 1

QUICK DETAIL:

 

DESCRIPTION:

HIGH IMPACT, HIGH FLOW

 

APPLICATIONS:

SKI FLAT, MISCELLANEOUS

 

SPECIFICATIONS:

N.W. 25KGS PER BAG, 40 BAGS PER PALLET.

 

COMPETITIVE ADVANTAGE:

1. RELIABILITY OF QUALITY

2. STABILITY OF SUPPLY

2. SHORTER LEAD TIME

3. COST-EFFECTIVENESS

4. TECHNICAL SUPPORT (INCLUDING INJECTION MOLDING, VIRTUE CAE SERVICES, ETC.)

5. VALUE ADDED SERVICE(INCLUDING PLASTIC COLOR MATCHING)

6. CUSTOMIZATION SERVICE TO MEET CUSTOMER'S REQUIREMENT.

 

 

Properties

Method

Unit

SH625

Physical

 

Specific Gravity , 23℃

ASTM D792

 

1.04

Mold Shrinkage , 23℃, 3.2mm , 23℃

ASTM D955

%

0.4 ~ 0.7

Melt Flow Rate , 220℃, 10kg

ASTM D1238

g/10min

7

Mechanical

 

Tensile Strength at Yield , 23℃, 50mm/min, 3.2mm

ASTM D638

Mpa

34

Tensile Elongation at Yield , 23℃, 50mm/min, 3.2mm

ASTM D638

%, (Min)

5

Tensile Elongation at Break , 23℃, 50mm/min, 3.2mm

ASTM D638

%, (Min)

15

Tensile Modulus , 23℃, 50mm/min, 3.2mm

ASTM D638

MPa

1250

Flexural Strength , 23℃, 15mm/min, 3.2mm

ASTM D790

Mpa

49

Flexural Modulus , 23℃, 15mm/min, 3.2mm

ASTM D790

MPa

1450

Izod Impact Strength , Notched, 3.2mm, 23℃

ASTM D256

J/m

540

Izod Impact Strength , Notched, 3.2mm, -30℃

ASTM D256

J/m

250

Izod Impact Strength , Notched, 6.4mm, 23℃

ASTM D256

J/m

460

Izod Impact Strength , Notched, 6.4mm, -30℃

ASTM D256

J/m

210

Rockwell Hardness , R-Scale

ASTM D785

 

95

Thermal

 

HDT , Edgewise, 1.82MPa, 6.4mm, Unannealed

ASTM D648

85

VICAT , 50N, 50℃/h

ASTM D1525

90

 

Note:

Typical values can be used only for the purpose of selecting material, and there can be variation within normal tolerances for various colors.Values given should not be interpreted as specification and not be used for designing part or tool.All properties, except melt flow rate are measured by injection molded specimens after 48 hours storage at 23℃, 50% relative humidity

ABS SH625 with High Flow and High Impact for Ski Flat, Miscellaneous goods,Refrigerator plate, suitcase, bobbin. 2

Processing Guide (Extrusion Molding)

Processing Parameters

Unit

Value

Drying Temperature

70 ~ 80

Drying Time

hrs

3 ~ 4

Minimum Moisture Content

%

0.01 ~ 0.01

Melt Temperature

200 ~ 250

Barrel Temperature, Zone 1

180 ~ 210

Barrel Temperature, Zone 2

190 ~ 230

Barrel Temperature, Zone 3

200 ~ 250

Barrel Temperature, Zone 4

200 ~ 250

Adapter Temperature

200 ~ 250

Die Temperature

200 ~ 250

Roll Stack Temperature, Top

70 ~ 100

Roll Stack Temperature, Middle

70 ~ 90

Roll Stack Temperature, Bottom

60 ~ 90

 

Note

Recommend initial lower temperatures settings to avoid material degradation/hang-up in die & purge material from extruder prior to shutdown.

Contact Details
EVER BEST(HK) LIMITED

Contact Person: Mr. Michael Zhu

Tel: +86 158 6238 0120

Send your inquiry directly to us (0 / 3000)

Other Products
Request A Quote

E-Mail | Sitemap

Privacy Policy China Good Quality ABS Plastic Raw Material Supplier. Copyright © 2020 - 2021 polymer-plastic.com. All Rights Reserved. Developed by ECER