One-stop sourcing for global plastic customers.
Become solution partner for our customers.
Place of Origin: | Korea |
Brand Name: | LG CHEM |
Certification: | MSDS, ROHS,UL, REACH |
Model Number: | SEETEC H7630 |
Minimum Order Quantity: | 18T |
---|---|
Price: | NEGOTIABLE ACCORDING TO ORDER QUANTITY |
Packaging Details: | 25KG/BAG, 40BAGS PER PALLET |
Delivery Time: | 30 WOKING DAYS UPON RECEIPT OF ORDER CONFIRMATION AND PAYMENT |
Payment Terms: | T/T |
Supply Ability: | 500T PER MONTH |
Material: | PP Homopolymer | Form: | Granules |
---|---|---|---|
Color: | Natural Color | Description: | Anti-gas Fading Stabilization |
Application: | Hygiene, Medical And Industrial | Grade: | Extrusion Molding Grade |
High Light: | pp plastic raw material,polypropylene granules |
PP Resin SEETEC H7630 Extrusion Molding Grade Plastic Raw Material with Very Narrow Molecular Weight Distribution(MWD) and Anti-gas Fading Stabilization for Hygiene, Medical and Industrial.
SEETEC H7630 Quick Detail:
1.Very Narrow Molecular Weight Distribution(MWD)
2.Anti-gas Fading Stabilization
SEETEC H7630 Description:
SÉETEC H7630 is designed for the extrusion of fine fibers with the spun bond technology. This grade is characterized by very narrow molecular weight distribution(MWD), with anti-gas fading stabilization.
SEETEC H7630 Applications:
Hygiene, Medical and Industrial.
SEETEC H7630 Datasheet:
Typical properties | |||
Characteristics | Test Method | Unit | Value |
Physical(1) | |||
Density | ASTM D1505 | g/㎤ | 0.9 |
MFR(230℃,2.16Kg) | ASTM D1238 | g/10min | 34 |
Mechanical(2) | |||
Tensile Strength at Yield | ASTM D638(3) | Mpa | 34 |
Elongation at Break | ASTM D638(3) | % | >500 |
Flexural Modulus | ASTM D790(4) | Mpa | 1600 |
Izod Impact Strength (Notched, 23℃) | ASTM D256 | J/m | 29 |
Hardness(R-scale) | ASTM D785 | - | 105 |
Thermal | |||
Vicat Softening point (1kgf) | ASTM D1525 | ℃ | 151 |
Heat Deflection Temperature (4.6kgf/cm2) | ASTM D648 | ℃ | 110 |
SEETEC H7630 Caution:
1. AVOID DIRECT SUNLIGHT, STORE IN COOL, DRY VENTILATED AREA.
2. KEEP AWAY FROM THE HEAT, SPARK, AND FLAME.
3. DO NOT INHALE GASEMITTED FROM THE HEATED RESIN.
4. DIRECT CONTACT WITH THE MELTED RESIN MAY CAUSE SEVERE BURNS.
5. THE WORKSHOP FLOOR SHOULD BE KEPT CLEAN AT ALL TIMES IN ORDER TO PREVENT ACCIDENT ASSOCIATED WITH LOOSE PELLETS OR FILM.
6. LIFTING OF HEAVY BAGS CAN CAUSE DAMAGE TO YOUR SPINE IF NOT DONE CORRECTLY